Introduction
The model-free analysis according to ASTM E2070 is an isoconversional method only for isothermal data. At least two measurements at different isothermal temperatures are required.
The determination of the activation energy is using the points at the same conversion (0.01, 0.02, …, 0.99, 1.00) from the measurements at different isothermal temperatures. There is no assumption about the reaction type.
In the following example, conversion data for the isothermal crystallization of a polymer are shown, where the crystallization process is faster the lower the temperature is (103.5°C: orange; 103.0°C: cyan; 102.5°C: red).
Activation energy and pre-exponential are found from the slope and intersect of these lines.
Advantage of this method: each reaction point is evaluated.
Disadvantages of this method:
- only one-step reactions, for complex reactions the points are not on the straight line;
- only for the set of several isothermal measurements;
Method Source: ASTM 2070, Method A. https://www.astm.org/Standards/E2070.htm
Here three isothermal measurements are done for the isothermal crystallization of LDPE:
- 102.5°C,
- 103.0°C
- 103.5°C.
NOTE: If you work with your own data, and these data do not start from time=0, then please select the range of isothermal data only where the left border of selected range corresponds to the reaction start.
Analysis shows graphic Log of time-to-conversion vs inverse temperature for the points with the same conversion from the different measurements. The graphic shown as the straight line for each conversion value.
For isothermal chemical reactions the slope of these lines is positive, because the reaction rate increases with the temperature. But here for isothermal crystallization the slope of the straight lines is negative because crystallization rate decreases with temperature.
6. Show activation energy and pre-exponential factor, which are calculated according to ASTM E2070.
Click on "Activation Energy" button to show Activation Energy chart.
Isothermal Lifetime Prediction
7. Select prediction and set prediction parameters.
In the left tree select Simulation → Prediction → Isothermal Lifetime.
In the prediction properties panel select ASTM E2070 model.
Set the prediction parameters:
- Minimal Temperature to 100°C,
- Maximal Temperature to 104°C,
- Temperature Step=1 min,
- Time for prediction is 100 min.
8. Press Calculate.
This graphic shows crystallization time for each given degree of crystallization for different temperatures. Each line presents one selected degree of conversion. E.g. the upper line here means the time for crystallization of 98% at different temperatures.
Temperatures are shown in the legend.
We see that:
- 98% of crystallization at 100°C happens after 9 min,
- 98% of crystallization at 104°C is reached after 40 min.
In order to see the predicted time values, please use Export Data on the main top toolbar.